Polymer Property : Hot Wire Ignition, HWI = 14 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.710 mm
7.0 - 14 sec

@Thickness 0.0280 in
UL 746
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746A
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM
Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R533 NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533 NT is general-purpose, 33% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade that is lubricated for good machine feed, flow and mold release. Gl..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R540H Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540H is general-purpose, heat-stabilized, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials VYDYNE® R543 Nylon, 43% Glass Reinforced, DAM
Vydyne® R543 is general purpose, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fee, flow and mold release. Glass..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.710 mm
7.0 - 14 sec

@Thickness 0.0280 in
UL 746A
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746A
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 1.50 mm
7.0 - 14 sec

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 3.00 mm
7.0 - 14 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..