Polymer Property : Comparative Tracking Index = 399 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Comparative Tracking Index 125 - 399 V
125 - 399 V
Average value: 179 V Grade Count:28
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 18 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 19 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 24 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 24 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 25 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 27 U Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® F 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® FC 19 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® FC 22 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® MX 1000 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Comparative Tracking Index 250 - 399 V
250 - 399 V
IEC Pub1.112, class 2; IEC Method
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
Comparative Tracking Index 250 - 399 V
250 - 399 V
IEC Pub1.112, class 2; IEC Method
Toyobo VYLOPET® EMC407 Non-Reinforced
Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessImproved processabilityHigh fluidityGood appearanceInformation provided by Toyobo.
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Dry as Molded
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
Comparative Tracking Index 250 - 399 V

@Thickness 3.05 mm
250 - 399 V

@Thickness 0.120 in
UL PLC 2 (250-399 V)
Resinoid 1312 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Comparative Tracking Index 250 - 399 V

@Thickness 3.00 mm
250 - 399 V

@Thickness 0.118 in
IEC 60112
Ascend Performance Materials Vydyne® R533H NAT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NAT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
Mitsubishi Xantar® 27 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..
Comparative Tracking Index 250 - 399 V
250 - 399 V
PLC 2; UL 746A
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..