Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 1.10 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Polykemi AB SCANAMID 66 A32^E Nylon 66, Modified
Information provided by Polykemi AB
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A HSX88 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K-FHG6 (Dry) 30% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® Ultraflow™ K-FKGS6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Cond)  (discontinued *
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Styrolution Luran® S KR 2864 C UV Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis MG7547S Polyethylene
MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
cond; ISO 179/1eA
DSM Akulon® K224-G6-FC NA99001 PA6-GF30
30% Glass Reinforced, Food Contact Grade
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
cond; ISO 179/1eA
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30
30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4 sp=62; ISO 179/1eA
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded
BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Edgew 80x10x4; ISO 179/1eA
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179/eA
Eurotec® Tecomid® NA40 GR25 NL PA 6.6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Arkema Group Rilsamid® PA 12 AESNO MED Nylon 12
Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -40.0 °C
5.23 ft-lb/in²

@Temperature -40.0 °F
ISO 179
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher ..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.24 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned
Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled
SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Charpy Impact, Notched 1.10 J/cm²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, Conditioned
Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh..
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled
SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers