| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 4.00 hour | 4.00 hour | |
|
PolyOne OnForce™ LFT NN-60LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
|
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced
Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
|
|||
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
|
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance
Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid..
|
|||
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
|
LG Chemical LUMID HI5001AS PA6/PO, High Barrier Property, CaCl2 Resistance, High Impact
Feature: Injection Molding, PA6/PO, High Barrier Property, CaCl2 Resistance, High ImpactApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1, 9002-88-4 and 105-60-2Information pro..
|
|||
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
|
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface
Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
|
LG Chemical LUPOY GP5006B PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | DAM; Extrusion |
|
DuPont Performance Polymers Zytel® FN714 NC010A Nylon 66
Zytel® FN714 NC010A is an impact modified, very flexible, plasticizer free polyamide 66 resin having good heat aging and chemical resistance.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
|
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded
PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded
Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
Eurostar Starflam PW0042E PA6, 20% Mineral Filled, Injection Molded
PW0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Reinforced, Polyamide 6 Injection MoldingInformation provided by Polymer Technology & Services, the North American exclus..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
Eurotec® Tecomid® NT40 GR50 NL HS PPA, 50% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | Injection |
|
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | Extrusion |
|
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
Ascend Performance Materials Vydyne® R543H BK02 Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H BK02 is general-purpose, 43% glass-fiber reinforced PA66 resin. Available in black, it is an injection-molding grade resin that is lubricated for machine feed, flow and mold release. ..
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | |
|
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded
BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
|
|||
| Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour | Injection Molding |
|
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |
|
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical
|
|||
| Dry Time | 4.00 hour | 4.00 hour | |
|
DuPont Performance Polymers Rynite® FG530 NC011 PET
(Unverified Data**)
Rynite® FG530 NC011is a 30% glass fiber reinforced modified polyethylene terephthalate resin. It has been developed for consideration into applications for the food industry.Information provided by..
|
|||