| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.800 mm
|
7.0
-
15
sec <br>@Thickness 0.0315 in
|
UL 746 |
|
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical HG173 ABS, High Surface Gloss
Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=3.00 mm
|
7.0
-
15
sec <br>@Thickness >=0.118 in
|
|
|
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=0.750 mm
|
7.0
-
15
sec <br>@Thickness >=0.0295 in
|
|
|
LG Chemical LUPOL GP1000FC Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=0.820 mm
|
7.0
-
15
sec <br>@Thickness >=0.0323 in
|
|
|
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance
Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance
Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical XR401B ABS, High Flow, Heat Resistance
Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness >=1.50 mm
|
7.0
-
15
sec <br>@Thickness >=0.0591 in
|
|
|
LG Chemical XR401T ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R525H BK0201 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK0201 is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials VYDYNE® R533H Nylon, 33% Glass Reinforced, DAM
Vydyne® R533H is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when exposed to anti-free..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
15
sec <br>@Thickness 0.750 mm
|
7.0
-
15
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.710 mm
|
7.0
-
14
sec <br>@Thickness 0.0280 in
|
UL 746A |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 1.50 mm
|
7.0
-
14
sec <br>@Thickness 0.0591 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 3.00 mm
|
7.0
-
14
sec <br>@Thickness 0.118 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.400 mm
|
7.0
-
14
sec <br>@Thickness 0.0157 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R533H BK0201 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK0201 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||
| Hot Wire Ignition, HWI |
7.0
-
14
sec <br>@Thickness 0.750 mm
|
7.0
-
14
sec <br>@Thickness 0.0295 in
|
UL 746 |
|
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
|
|||