Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 °C @Time 14400 sec |
176 °F @Time 4.00 hour |
|
Plastcom PLASTAMID® 66 BT SD PA66 Basic type PA66 for injection molding, modified for general use. PA66 contains TiO2 up to 0.5% wt. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners,.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Drying Temperature | 80.0 °C @Time 14400 sec |
176 °F @Time 4.00 hour |
|
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
LG Chemical LUPOY GP5006AF PC/ABS, Flame Retardant Description: Injection Molding, PC/ABS, Flame RetardantApplication: Electric and Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chem.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 14400 sec |
176 °F @Time 2.00 - 4.00 hour |
Desiccant |
Metabolix Mirelâ„¢ P1003 Injection Molding Grade PHA Bioplastic Mirelâ„¢ P1003 is a general purpose injection molding material with high modulus.Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and .. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Gromax BFM40-DL04N1 Nylon 6 40% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers PA 66, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS. |
|||
Drying Temperature | 80.0 - 90.0 °C @Time 10800 sec |
176 - 194 °F @Time 3.00 hour |
|
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Chemical grafting Heat stabilized. Metal stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE freeAvailability: A.. |
|||
Drying Temperature | 80.0 - 100 °C @Time 10800 sec |
176 - 212 °F @Time 3.00 hour |
|
LATI Latigray 82-03 CW/96 F3 PA 12, Metallic Reinforced Radiopaque compound based on Polyamide 12 (PA12). Metallic filler. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America;.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 21600 sec |
176 °F @Time 2.00 - 6.00 hour |
|
Sax Polymers SAXAMID 126F6T3 Nylon 6, 30% Glass Fiber and PTFE SAXAMID 126F6T3 is a polyamide 6 injection-molding-grade reinforced with 30% glass fibers and 15% PTFE. Because of its high strength and stiffness this grade is often used for stressed parts requiri.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 21600 sec |
176 °F @Time 2.00 - 6.00 hour |
|
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | |
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in.. |
|||
Drying Temperature | 80.0 °C | 176 °F | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6 Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr.. |
|||
Drying Temperature | 80.0 °C | 176 °F | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Toluene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 80.0 °C | 176 °F | Option 1 |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 °C @Time 14400 sec |
176 °F @Time 4.00 hour |
|
Eurostar Starflam PX06011 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06011 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding Resin (also known as Starflam PF1005Z222)Information provided by Eurosta.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Eurotec® Tecomid® NA40 AR20 NL HS PA6.6, 20% aramid fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Drying Temperature | 80.0 °C | 176 °F | Extrusion |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Drying Temperature | 80.0 °C | 176 °F | |
Plastcom SLOVALEN PQ 83 T 40 PP, 40% mineral filling FeaturesModified PP for injection moulding with the content of 40% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Drying Temperature | 80.0 - 90.0 °C | 176 - 194 °F | Must be dried. Typical condition. |
BASF Elastollan® M88A15 Polyester Type Polyurethane Elastomer The Elastollan M Series of products listed are part of a new series of polyester-based thermoplastic polyurethanes (TPU). They are specifically formulated for fast cycling in Injection Molding appl.. |