Processing Properties Metric English Comments
Middle Barrel Temperature 280 - 300 °C
536 - 572 °F
Injection Molding
LG Chemical LUPOY GN1006FM PC, Halogen Free, Flame Retardant, Transparency
Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical
Middle Barrel Temperature 280 - 315 °C
536 - 599 °F
LG Chemical LUPOY GN-2151F Halogen Free Modified PC, 15% Glass Fiber Reinforced, Flame Retardant, Green
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Middle Barrel Temperature 280 - 300 °C
536 - 572 °F
Injection Molding
LG Chemical LUPOY GP1000HU PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, UV StabilityApplication: Electric & Electronic (Housing, Components) For Suit caseCAS: 103598-77-2Information provided by LG Chemic..
Middle Barrel Temperature 280 - 300 °C
536 - 572 °F
Injection Molding
LG Chemical LUPOY GP1000L PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Injection Molding
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Middle Barrel Temperature 280 - 315 °C
536 - 599 °F
LG Chemical LUPOY GP-2401F General Purpose Modified PC, 40% Glass Fiber Reinforced, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Injection Molding
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Injection Molding
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Middle Barrel Temperature 280 - 300 °C
536 - 572 °F
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Middle Barrel Temperature 280 - 300 °C
536 - 572 °F
Samyang Trirex® 3025A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R228 Nylon 66, 40% Mineral Reinforced, DAM
Vydyne® R228 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in black, it is an injection-molding grade formulated to retain the inherent processing advant..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R513H Black Nylon 66, 13% Glass Reinforced, DAM
Vydyne® R513H Black is general-purpose, 13% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is an injection-molding grade that is lubricated for machine feed, flow, and m..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM
Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H NT Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H NT is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties ..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM
Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
Middle Barrel Temperature 280 °C
536 °F
Beijing Chemical Industry KAIFA® M106N MPPO Resin
High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Injection Molding
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Middle Barrel Temperature 280 - 310 °C
536 - 590 °F
Ascend Performance Materials Vydyne® R533 Nylon 66, 33% Glass Filled, Dry as Molded
Vydyne® R533 is general-purpose, 33% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for good machine feed, flow, and mold release. Glas..
Copyright © lookpolymers.com All Rights Reserved