Overview of materials for Thermoplastic Olefinic Elastomer (TPO)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Olefinic Elastomer (TPO).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.850 - 1.82 g/cc
0.0307 - 0.0658 lb/in³
Average value: 1.00 g/cc Grade Count:381
Filler Content 10.0 - 30.0 %
10.0 - 30.0 %
Average value: 18.3 % Grade Count:9
Water Absorption 0.0100 - 0.0500 %
0.0100 - 0.0500 %
Average value: 0.0320 % Grade Count:15
Viscosity 102000 - 458000 cP

@Temperature 190 - 200 °C
102000 - 458000 cP

@Temperature 374 - 392 °F
Average value: 277000 cP Grade Count:29
102000 - 458000 cP

@Shear Rate 206 - 300 1/s
102000 - 458000 cP

@Shear Rate 206 - 300 1/s
Average value: 277000 cP Grade Count:29
Mooney Viscosity 6.50 - 19.0
6.50 - 19.0
Average value: 11.8 Grade Count:3
Environmental Stress Crack Resistance 1000 hour
1000 hour
Average value: 1000 hour Grade Count:4
Thickness 20.3 - 31.8 microns
0.800 - 1.25 mil
Average value: 24.1 microns Grade Count:3
Linear Mold Shrinkage 0.00100 - 0.0350 cm/cm
0.00100 - 0.0350 in/in
Average value: 0.0125 cm/cm Grade Count:219
0.00600 - 0.00900 cm/cm

@Temperature 80.0 - 121 °C
0.00600 - 0.00900 in/in

@Temperature 176 - 250 °F
Average value: 0.00750 cm/cm Grade Count:3
0.00600 - 0.00900 cm/cm

@Time 3600 - 3600 sec
0.00600 - 0.00900 in/in

@Time 1.00 - 1.00 hour
Average value: 0.00750 cm/cm Grade Count:3
Linear Mold Shrinkage, Transverse 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00900 cm/cm Grade Count:16
Melt Flow 0.500 - 42.0 g/10 min
0.500 - 42.0 g/10 min
Average value: 10.7 g/10 min Grade Count:249
Ash 0.000 - 34.0 %
0.000 - 34.0 %
Average value: 10.7 % Grade Count:14
19.0 - 19.0 %

@Temperature 600 - 950 °C
19.0 - 19.0 %

@Temperature 1110 - 1740 °F
Average value: 19.0 % Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell R 49.0 - 95.0
49.0 - 95.0
Average value: 79.1 Grade Count:16
Hardness, Shore A 33.0 - 95.0
33.0 - 95.0
Average value: 68.1 Grade Count:130
Hardness, Shore D 11.0 - 95.0
11.0 - 95.0
Average value: 53.5 Grade Count:184
Ball Indentation Hardness 33.0 - 43.0 MPa
4790 - 6240 psi
Average value: 35.6 MPa Grade Count:7
Tensile Strength, Ultimate 0.689 - 57.0 MPa
100 - 8270 psi
Average value: 11.3 MPa Grade Count:258
Film Tensile Strength at Yield, MD 2.95 - 5.40 MPa
428 - 783 psi
Average value: 4.50 MPa Grade Count:4
Film Tensile Strength at Yield, TD 3.24 - 5.20 MPa
470 - 754 psi
Average value: 4.34 MPa Grade Count:4
Tensile Strength, Yield 1.00 - 33.0 MPa
145 - 4790 psi
Average value: 12.5 MPa Grade Count:220
Film Elongation at Break, MD 410 - 460 %
410 - 460 %
Average value: 438 % Grade Count:4
Film Elongation at Break, TD 480 - 820 %
480 - 820 %
Average value: 645 % Grade Count:4
Elongation at Break 8.00 - 2000 %
8.00 - 2000 %
Average value: 443 % Grade Count:297
Elongation at Yield 4.00 - 525 %
4.00 - 525 %
Average value: 40.0 % Grade Count:67
Modulus of Elasticity 0.000986 - 2.10 GPa
0.143 - 305 ksi
Average value: 0.583 GPa Grade Count:31
Flexural Yield Strength 3.45 - 68.9 MPa
500 - 10000 psi
Average value: 22.2 MPa Grade Count:32
Flexural Modulus 0.00540 - 4.60 GPa
0.783 - 667 ksi
Average value: 0.967 GPa Grade Count:233
Secant Modulus 0.0310 - 0.239 GPa
4.50 - 34.7 ksi
Average value: 0.101 GPa Grade Count:10
Secant Modulus, MD 0.0343 - 0.0719 GPa
4.97 - 10.4 ksi
Average value: 0.0522 GPa Grade Count:4
Secant Modulus, TD 0.0359 - 0.0744 GPa
5.20 - 10.8 ksi
Average value: 0.0552 GPa Grade Count:4
Izod Impact, Notched 0.395 J/cm - NB
0.740 ft-lb/in - NB
Average value: 4.34 J/cm Grade Count:89
0.42712 - 7.68816 J/cm

@Temperature -40.0 - -18.0 °C
0.80017 - 14.4031 ft-lb/in

@Temperature -40.0 - -0.400 °F
Average value: 1.66 J/cm Grade Count:31
Izod Impact, Unnotched 6.94 - 5340 J/cm
13.0 - 10000 ft-lb/in
Average value: 6.94 J/cm Grade Count:14
Izod Impact, Notched (ISO) 3.80 kJ/m² - NB
1.81 ft-lb/in² - NB
Average value: 34.5 kJ/m² Grade Count:41
1.10 kJ/m² - NB

@Temperature -40.0 - 10.0 °C
0.523 ft-lb/in² - NB

@Temperature -40.0 - 50.0 °F
Average value: 8.84 kJ/m² Grade Count:32
Izod Impact, Unnotched (ISO) 46.0 - 48.0 kJ/m²
21.9 - 22.8 ft-lb/in²
Average value: 46.7 kJ/m² Grade Count:3
Charpy Impact Unnotched 4.50 J/cm² - NB
21.4 ft-lb/in² - NB
Average value: 20.8 J/cm² Grade Count:18
4.50 J/cm² - NB

@Temperature -40.0 - -20.0 °C
21.4 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 18.0 J/cm² Grade Count:15
Charpy Impact, Notched 1.30 - 6.50 J/cm²
6.19 - 30.9 ft-lb/in²
Average value: 4.07 J/cm² Grade Count:15
0.200 - 1.00 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.508 J/cm² Grade Count:15
Gardner Impact 4.90 J - NB
3.61 ft-lb - NB
Average value: 56.5 J Grade Count:67
1.00 - 48.0 J

@Temperature -30.0 - -30.0 °C
0.738 - 35.4 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 27.9 J Grade Count:73
Dart Drop, Total Energy 16.0 - 18.0 J
11.8 - 13.3 ft-lb
Average value: 16.7 J Grade Count:3
17.0 - 25.0 J

@Temperature -30.0 - 0.000 °C
12.5 - 18.4 ft-lb

@Temperature -22.0 - 32.0 °F
Average value: 22.6 J Grade Count:20
Tear Strength 7.01 - 550 kN/m
40.0 - 3140 pli
Average value: 65.3 kN/m Grade Count:158
Graves Tear Strength 14.2 - 52.6 kN/m
81.0 - 300 pli
Average value: 28.7 kN/m Grade Count:12
Elmendorf Tear Strength, MD 2.56 - 12.2 g/micron
65.0 - 310 g/mil
Average value: 8.46 g/micron Grade Count:3
Elmendorf Tear Strength, TD 4.92 - 25.2 g/micron
125 - 640 g/mil
Average value: 16.6 g/micron Grade Count:3
Dart Drop 22.4 - 57.1 g/micron
570 - 1450 g/mil
Average value: 42.4 g/micron Grade Count:3
Taber Abrasion, mg/1000 Cycles 10.0 - 189
10.0 - 189
Average value: 89.2 Grade Count:9
Compression Set 10.0 - 79.0 %
10.0 - 79.0 %
Average value: 30.2 % Grade Count:59
33.0 - 95.0 %

@Temperature 70.0 - 100 °C
33.0 - 95.0 %

@Temperature 158 - 212 °F
Average value: 53.4 % Grade Count:52
27.0 - 57.0 %

@Temperature 70.0 - 100 °C
27.0 - 57.0 %

@Temperature 158 - 212 °F
Average value: 53.4 % Grade Count:8
27.0 - 57.0 %

@Time 79200 - 79200 sec
27.0 - 57.0 %

@Time 22.0 - 22.0 hour
Average value: 53.4 % Grade Count:8
Tensile Set 3.40 - 16.0 %
3.40 - 16.0 %
Average value: 8.54 % Grade Count:12
Users viewing this material also viewed the following: