Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | ASTM D256 |
Network Polymers Kepital® TC30-20 Description: Natural Acetal Copolymer, 10% Talc Reinforced GradeInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.395 J/cm - NB | 0.740 ft-lb/in - NB | Average value: 4.34 J/cm Grade Count:89 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | CB; ASTM D256A |
Solvay Engineered Polymers INDURE™ E1500 HG TPO
(discontinued **) Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material.. |
|||
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | CB; ASTM D256A |
Solvay Engineered Polymers INDURE™ E1600 TPO
(discontinued **) Description: INDURE™ E1600 is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material is.. |
|||
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | ASTM D256 |
LyondellBasell Alathon® H6017 High Density Polyethylene, Injection Molding Grade ALATHON H6017 provides good processing characteristics and exhibits excellent toughness and color as well as low odor and good molded-part stability. Typical applications include housewares, caps, c.. |
|||
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® XP-91 Compression Molded PEEK Compound, 30% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Izod Impact, Notched | 0.395 J/cm | 0.740 ft-lb/in | ASTM D256A |
ExxonMobil PP5722E1 Polypropylene Copolymer Product Description: A medium flow homopolymer resin designed for mono-oriented products like stretched tapes and monofilament.Availability: Asia Pacific Features:Good Gauge ControlGood Processabil.. |