Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00540 - 4.60 GPa | 0.783 - 667 ksi | Average value: 0.967 GPa Grade Count:233 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Modulus | 3.40 - 4.60 GPa | 493 - 667 ksi | Average value: 4.20 GPa Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |