Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.850 g/cc | 0.0307 lb/in³ | |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Density | 0.850 - 1.82 g/cc | 0.0307 - 0.0658 lb/in³ | Average value: 1.00 g/cc Grade Count:381 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Density | 0.850 - 2.28 g/cc | 0.0307 - 0.0824 lb/in³ | Average value: 2.01 g/cc Grade Count:24 |
Overview of materials for Polytetrafluoroethylene (PTFE) Powder This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Density | >= 0.850 g/cc @Temperature 20.0 °C |
>= 0.0307 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-10 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.850 - 1.00 g/cc @Temperature 20.0 °C |
0.0307 - 0.0361 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez Pyrolysis Heavy Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis. Application: Used in the production of technical carbon, coak, and dark polymeric petroleum resin.Informa.. |
|||
Density | 0.851 - 0.887 g/cc | 0.0307 - 0.0320 lb/in³ | |
Lord Adhesives 459X Xylene Adhesion Promoter for Lord Acrylic, Epoxy, Urethane and Cyanoacrylate Adhesives Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.850 - 0.8747 g/cc | 0.0307 - 0.03160 lb/in³ | Chemlok® 485 |
Lord Adhesives Chemlok® 485/Curative 44 Adhesive LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers.. |
|||
Density | 0.850 - 0.870 g/cc @Temperature 15.0 °C |
0.0307 - 0.0314 lb/in³ @Temperature 59.0 °F |
|
Unipetrol BTX fraction BTX fraction is manufactured by distillation of pyrolysis petrol. It is yellowish, highly combustible and easily inflammable liquid with strong aromatic odour. BTX fraction is mixture of aromatic hy.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
Thermoseal soft-chem® PTFE Gasketing Thermoseal® soft-chem® expanded PTFE sealing material provides excellent corrosion resistance and impermeability along with superior creep resistance and sealability for use in all types of applic.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac Synthetic ATF Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf.. |
|||
Density | 0.849 g/cc @Temperature 15.6 °C |
0.0307 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Elite™ 150 Metallocene Polyalphaolefin (mPAO) Fluid Product Description: SpectraSyn ™ metallocene Polyalphaolefin (mPAO) basestock is an advanced high viscosity (Hi-Vis) Polyalphaolefin (PAO). SpectraSyn ™ mPAO utilized metallocene catalyst technol.. |
|||
Density | 0.850 g/cc @Temperature 15.6 °C |
0.0307 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn™ 40 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ISO 12185 |
ExxonMobil Varsol™ 140 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.851 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 0W-30 Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
ConocoPhillips Hydroclear® 70 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
ConocoPhillips Hydroclear® 90 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.850 g/cc @Temperature 15.6 °C |
0.0307 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Ultra™ 150 High VI Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high visco.. |
|||
Density | 0.849 - 0.913 g/cc | 0.0307 - 0.0330 lb/in³ | |
CMT Materials HYTAC® WF High Strength High Clarity 450°F Epoxy Syntactic HYTAC-WF is an excellent high temperature epoxy syntactic material that provides improved clarity when forming APET and other clear polymers plus reduces sticking of difficult to process polymers su.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF Lupragen® 205 Bix(2-Dimethylaminoethyl)ether Formula: C8H20N2OCAS: 3033-62-3Description: Bis(2-Dimethylaminoethyl)ether is a colorless to yellowish liquid, with an amine-like odor. It is also miscible with water.Synonyms: BDMAEE, N,N,N’,N’-.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
BASF N,N-Dimethylisopropanolamine Formula: C5H13NOCAS: 108-16-7Description: Dimethylisopropanolamine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: Dimethylisopropanolamine, 1-Dimethylami.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac Synthetic ATF Mobil Delvac Synthetic ATF is a synthetic fluid designed that meets the demanding requirements of modern heavy duty automatic transmissions. The synthetic baseoil composition enables excellent perf.. |
|||
Density | 0.850 - 1.90 g/cc | 0.0307 - 0.0686 lb/in³ | Average value: 1.09 g/cc Grade Count:250 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 0.850 g/cc | 0.0307 lb/in³ | |
LATI Latimass 53-04 D009 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Density | 0.850 g/cc @Temperature 15.0 °C |
0.0307 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 797 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.849 g/cc | 0.0307 lb/in³ | |
BNZ Materials 2653LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |