Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Temperature 80.0 - 121 °C
0.00600 - 0.00900 in/in

@Temperature 176 - 250 °F
Average value: 0.00750 cm/cm Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Time 3600 - 3600 sec
0.00600 - 0.00900 in/in

@Time 1.00 - 1.00 hour
Average value: 0.00750 cm/cm Grade Count:3
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Linear Mold Shrinkage 0.000 - 0.00900 cm/cm
0.000 - 0.00900 in/in
Average value: 0.00184 cm/cm Grade Count:17
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00291 cm/cm Grade Count:52
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00508 cm/cm Grade Count:111
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00321 cm/cm Grade Count:56
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00256 cm/cm Grade Count:72
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00177 cm/cm Grade Count:44
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00517 cm/cm Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "ABS + Glass Blend". Each property range of values reported is minimum and maximum values of appropriate ..
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00655 cm/cm Grade Count:33
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Linear Mold Shrinkage 0.00100 - 0.00900 cm/cm
0.00100 - 0.00900 in/in
Average value: 0.00700 cm/cm Grade Count:14
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
Linear Mold Shrinkage 0.000200 - 0.00900 cm/cm
0.000200 - 0.00900 in/in
Average value: 0.00341 cm/cm Grade Count:110
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00557 cm/cm Grade Count:55
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00281 - 0.00900 cm/cm
0.00281 - 0.00900 in/in
Average value: 0.00522 cm/cm Grade Count:21
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.000500 - 0.00900 cm/cm
0.000500 - 0.00900 in/in
Average value: 0.00262 cm/cm Grade Count:34
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00639 cm/cm Grade Count:25
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 1099 X 138299 Polybutylene Terephthalate (PBT) Glass Fiber - Flame Retardant - Halogen Free
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cm
0.00200 - 0.00900 in/in
Average value: 0.00491 cm/cm Grade Count:7
Overview of materials for Polypropylene with Glass Fiber + Bead Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Temperature 80.0 - 121 °C
0.00600 - 0.00900 in/in

@Temperature 176 - 250 °F
Average value: 0.00750 cm/cm Grade Count:1
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Time 3600 - 3600 sec
0.00600 - 0.00900 in/in

@Time 1.00 - 1.00 hour
Average value: 0.00750 cm/cm Grade Count:1
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 399 X 138765 U Polycarbonate (PC) ESD Protection - Permanently Static Dissipative - UV Stabilized
This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.
Linear Mold Shrinkage 0.00300 - 0.00900 cm/cm
0.00300 - 0.00900 in/in
Average value: 0.00600 cm/cm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Linear Mold Shrinkage 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00580 cm/cm Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 2099 X 134514 Polycarbonate/Polyester Flame Retardant - UV Stabilized - Chemical Resistant Alloy
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 300 UV Polycarbonate (PC), UV Stabilized
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 399 X 129955 E Polycarbonate (PC), Flame Retardant - Transparent
Linear Mold Shrinkage 0.00600 - 0.00900 cm/cm

@Thickness 3.20 mm
0.00600 - 0.00900 in/in

@Thickness 0.126 in
ASTM D 955
RTP Company RTP 399 X 138754 C Polycarbonate (PC) Permanently Static Dissipative - ESD Protection - UV Stabilized
This compound has been formulated to meet the static dissipative requirements of the ATEX Directive.
Copyright © lookpolymers.com All Rights Reserved