Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer ABSN3BK ABS Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer ABSN4BK ABS Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PA66GI14BK Nylon 66, 14% Glass Fiber Filled, Impact Modified Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PCABSN10BK PC/ABS Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PCABSN8BK PC/ABS Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PCM12BK PC Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PCM18BK PC Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | ASTM D955 |
Niche Polymer PCM6BK PC Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 - 0.0100 cm/cm | 0.00600 - 0.0100 in/in | ASTM D955 |
Niche Polymer PPCT40BK Copolymer PP, 40% Talc Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Temperature 80.0 - 121 °C |
0.00600 - 0.00900 in/in @Temperature 176 - 250 °F |
Average value: 0.00750 cm/cm Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Time 3600 - 3600 sec |
0.00600 - 0.00900 in/in @Time 1.00 - 1.00 hour |
Average value: 0.00750 cm/cm Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.0212 cm/cm | 0.00600 - 0.0212 in/in | Average value: 0.0113 cm/cm Grade Count:105 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.0110 cm/cm | 0.00600 - 0.0110 in/in | Average value: 0.00900 cm/cm Grade Count:5 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.0180 cm/cm | 0.00600 - 0.0180 in/in | Average value: 0.0100 cm/cm Grade Count:9 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Temperature 80.0 - 121 °C |
0.00600 - 0.00900 in/in @Temperature 176 - 250 °F |
Average value: 0.00750 cm/cm Grade Count:1 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00900 cm/cm @Time 3600 - 3600 sec |
0.00600 - 0.00900 in/in @Time 1.00 - 1.00 hour |
Average value: 0.00750 cm/cm Grade Count:1 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Linear Mold Shrinkage | 0.00600 cm/cm | 0.00600 in/in | Average value: 0.00600 cm/cm Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |