Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1eA |
Mytex Polymers AS172LW-01US Thermoplastic Polyolefin, Compounded AS172LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
Izod Impact, Unnotched (ISO) | 46.0 - 48.0 kJ/m² | 21.9 - 22.8 ft-lb/in² | Average value: 46.7 kJ/m² Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1eA |
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP EFL36 PEI (Asia Pacific) LNP LUBRICOMP* EFL36 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP EFL36XXC PEI LNP* Lubricomp* EFL36XXC is a compound based on Polyetherimide containing 30% Glass Fiber, 155 PTFE. Characteristics of this grade are: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RCP36XXP PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCP36XXP is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RCP36XXQ PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RCP36XXQ is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Easy Molding, Internally Lu.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RFG16S PA 66 LNP* LUBRICOMP* RFG16S is a compound based on Nylon 66 resin containing 5% Graphite, 30% Glass Fiber. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RX06480 PA 66 LNP LUBRICOMP* RX06480 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 15% Lubricants. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT LNP LUBRICOMP* WFL34H is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT LNP LUBRICOMP* WFP36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific) LNP LUBRICOMP* WFP36 is a compound based on Polybutylene Terephalate resin containing Silicone, Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY RF203AXH PA 66 LNP* LUBRILOY* RF203AXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR40DL Polyphenylene Sulfide, Glass Fiber Reinforced Injection molding, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hGR50 Polyphenylene Sulfide, Glass Fiber Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006EXZ PA 66 LNP THERMOCOMP* RF006EXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature -30.0 °C |
21.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² @Temperature 23.0 °C |
21.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF006ESZ PA 66 LNP THERMOCOMP* RF006ESZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 46.0 kJ/m² | 21.9 ft-lb/in² | 80*10*4; ISO 180/1U |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |