Polymer Property : Tear Strength = 40.0 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE)
Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha..
Tear Strength <= 7.01 kN/m
<= 40.0 pli
ASTM D624
Parker Chomerics CHO-SEAL® 6308 Conductive Elastomer
Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Extruded onlyRoHS CompliantInformation..
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu..
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer
Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil..
Tear Strength 7.01 - 550 kN/m
40.0 - 3140 pli
Average value: 65.3 kN/m Grade Count:158
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Tear Strength 7.01 kN/m
40.0 pli
Warp/Longitudinal direction
Saint-Gobain Chemlam® RL® RL4000 PTFE-Coated Non-woven Aramid Reinforced Laminate
Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint..
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE
Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
Tear Strength 7.01 kN/m
40.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2300-5R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications..
Tear Strength 7.01 kN/m
40.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2302-5R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications..
Tear Strength 7.01 kN/m
40.0 pli
Dow Corning SILASTIC® 9252/250P PARTS A&B
Information provided by Dow Corning
Tear Strength 7.01 kN/m
40.0 pli
Dow Corning SILASTIC® LCS-740 SILICONE RUBBER
40 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning
Tear Strength 7.01 kN/m
40.0 pli
Side 1, Silicone Property; ASTM D624
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot..
Tear Strength 7.01 kN/m
40.0 pli
Side 1, Silicone Property; ASTM D624
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat..
Tear Strength 7.01 kN/m
40.0 pli
Side 1, Silicone Property; ASTM D624
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene..
Tear Strength 7.01 kN/m
40.0 pli
Side 1 Silicone Property; ASTM D624
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material ..
Tear Strength 7.01 kN/m
40.0 pli
Side 1, Silicone Property; ASTM D624
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater..
Tear Strength 7.01 kN/m
40.0 pli
Layer 2, Silicone Property; ASTM D624
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..