Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
PolyOne Versaflex™ CL2003X Thermoplastic Elastomer (TPE) Versaflex™ CL2003X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and ultra-soft properties are desired. New Product. Commercial specifications ha.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Fill/Transverse direction |
Saint-Gobain Chemlam® RL® RL6000 PTFE-Coated Polyester/Cotton Blend Reinforced Laminate The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sintered PTFE for.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-1000 TPE Product Description: StarGrip GP 25-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2300-5R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 2 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2302-5R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 9030 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | D-470 |
Elastomer Engineering E850-85A Polyurethane A very tough and cut-resistant polyether-based formulation with good dynamic properties that bonds well to all metals. Information provided by Elastomer Engineering Inc (EEI) |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Trouser, PVC (70)/CP80AS2(30) |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | |
Dow Corning SILASTIC® 9252/250P PARTS A&B Information provided by Dow Corning |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Side 1, Silicone Property; ASTM D624 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Side 1, Silicone Property; ASTM D624 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Side 2, Layer 1, Silicone Property; ASTM D624 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Side 1 Silicone Property; ASTM D624 |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Side 1, Silicone Property; ASTM D624 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Tear Strength | 7.01 kN/m | 40.0 pli | Layer 2, Silicone Property; ASTM D624 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Tear Strength | >= 7.01 kN/m | >= 40.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Tear Strength | 7.01 - 1050 kN/m | 40.0 - 5990 pli | Average value: 147 kN/m Grade Count:115 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |