Material Notes:
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 8.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Flexural Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 0.240 J/cm

@Temperature 22.8 °C
0.450 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
Unannealed; ASTM D648
Vicat Softening Point 148 °C
298 °F
Loading 1 (10N); ASTM D1525