Mechanical Properties Metric English Comments
Gardner Impact 1.00 - 48.0 J

@Temperature -30.0 - -30.0 °C
0.738 - 35.4 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 27.9 J Grade Count:73
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Gardner Impact 1.00 J
0.738 ft-lb
ASTM D3029
Flint Hills P4G4K-038 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsma..
Gardner Impact 1.00 J

@Temperature -30.0 °C
0.738 ft-lb

@Temperature -22.0 °F
ASTM D5420
Flint Hills P5L2K-055 Polypropylene Random Copolymer
Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin..
Gardner Impact 1.00 J
0.738 ft-lb
ASTM D3029
Flint Hills P9H9Z-018 Polypropylene
Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Gardner Impact 1.00 - 36.6 J
0.738 - 27.0 ft-lb
Average value: 13.4 J Grade Count:11
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Gardner Impact 1.00 - 1.00 J

@Temperature -30.0 - -30.0 °C
0.738 - 0.738 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J Grade Count:1
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..
Gardner Impact 1.00 - 1.00 J

@Temperature -30.0 - -30.0 °C
0.738 - 0.738 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.00 J Grade Count:1
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..
Gardner Impact 1.00 - 36.0 J

@Temperature -30.0 - -20.0 °C
0.738 - 26.6 ft-lb

@Temperature -22.0 - -4.00 °F
Average value: 19.8 J Grade Count:41