Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 4.92 - 25.2 g/micron | 125 - 640 g/mil | Average value: 16.6 g/micron Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Elmendorf Tear Strength, TD | 4.92 g/micron | 125 g/mil | Cast Film at 1.25 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 4553 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceLow coefficient of friction Applications: .. |
|||
Elmendorf Tear Strength, TD | 4.92 g/micron | 125 g/mil | Blown Film at 1.25 mil; ASTM D-1922 |
Chevron Phillips MarFlex® 4571 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for cast film applications that require: High speed extrusionLow neck-inGood drawdownEdge tear resistanceHigh coefficient of friction Applications:.. |