Polymer Property : Ball Indentation Hardness = 4790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data)
TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C.
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)
TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa..
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data)
TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an..
Ball Indentation Hardness 33.0 - 43.0 MPa
4790 - 6240 psi
Average value: 35.6 MPa Grade Count:7
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Ball Indentation Hardness 33.0 MPa
4790 psi
132 N/10 s; ISO 2039
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-S15 PTFE
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 33.0 MPa
4790 psi
H385/30; ISO 2039
Borealis Daplen™ ED135AI TPO Compound
Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in..