Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 399L60 LDPE/Hexene Premium Blown Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 399L60 resin have balanced tensile, impact strength,.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
Dow DOWLEX™ 2047G Linear Low Density Polyethylene For high performance stretch film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Thickness | 20.3 microns | 0.800 mil | |
Dow DOWLEX™ 2078G Linear Low Density Polyethylene Good processability at narrow die gaps High strength in food applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Thickness | 20.3 microns | 0.800 mil | |
Dow DOWLEX™ 2021D Linear Low Density Polyethylene Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Thickness | 20.3 microns | 0.800 mil | |
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7741 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
3M 4492W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7733FLW Overlaminating Film 3M™ Overlaminating Film 7733FLW utilizes a clear polyester film that is recommended for optimum durability and superior outdoor UV exposure and print fade protection. 3M™ Adhesive 400 offers excel.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7776 Polypropylene Label Material 3M™ Polypropylene Label Material 7776 is a durable polypropylene label stock that offers excellent performance in applications requiring surface conformability. This label product utilizes 3M™ Adh.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Thickness | 20.3 microns | 0.800 mil | Adhesive |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Thickness | 20.3 microns | 0.800 mil | |
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |