Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.80 kJ/m² - NB | 1.81 ft-lb/in² - NB | Average value: 34.5 kJ/m² Grade Count:41 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched (ISO) | 3.80 - 23.0 kJ/m² | 1.81 - 10.9 ft-lb/in² | Average value: 6.79 kJ/m² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Izod Impact, Notched (ISO) | 3.80 - 16.0 kJ/m² | 1.81 - 7.61 ft-lb/in² | Average value: 7.07 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² | 1.81 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Star L PA6 D36 PA6, Injection Molded Star L PA6 D36 is a MOS2 Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² | 1.81 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² | 1.81 ft-lb/in² | ISO Test |
BASF Ultramid® 8231G HS BK-106 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-106 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² | 1.81 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NCFA Homopolymer 20% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Izod Impact, Notched (ISO) | 3.80 kJ/m² | 1.81 ft-lb/in² | ISO Test |
BASF Ultramid® B3GM35 BKQ649 23220 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 BKQ649 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |
|||
Izod Impact, Notched (ISO) | 3.80 - 12.0 kJ/m² | 1.81 - 5.71 ft-lb/in² | Average value: 6.65 kJ/m² Grade Count:18 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |