Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 4790 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.00 - 33.0 MPa
145 - 4790 psi
Average value: 12.5 MPa Grade Count:220
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Tensile Strength, Yield 9.00 - 33.0 MPa
1310 - 4790 psi
Average value: 26.5 MPa Grade Count:6
Overview of materials for Nylon 612, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app..
Tensile Strength, Yield 15.0 - 33.0 MPa
2180 - 4790 psi
Average value: 25.1 MPa Grade Count:14
Overview of materials for Nylon 11, Flexible Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o..
Copyright © lookpolymers.com All Rights Reserved