Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.500 - 42.0 g/10 min | 0.500 - 42.0 g/10 min | Average value: 10.7 g/10 min Grade Count:249 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Melt Flow | 0.100 - 42.0 g/10 min | 0.100 - 42.0 g/10 min | Average value: 9.51 g/10 min Grade Count:177 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Melt Flow | 0.100 - 42.0 g/10 min | 0.100 - 42.0 g/10 min | Average value: 7.62 g/10 min Grade Count:26 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 0.300 - 42.0 g/10 min | 0.300 - 42.0 g/10 min | Average value: 15.1 g/10 min Grade Count:15 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Melt Flow | 0.200 - 42.0 g/10 min | 0.200 - 42.0 g/10 min | Average value: 7.67 g/10 min Grade Count:125 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |