Mechanical Properties Metric English Comments
Graves Tear Strength 14.2 - 52.6 kN/m
81.0 - 300 pli
Average value: 28.7 kN/m Grade Count:12
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..
Graves Tear Strength 14.2 kN/m

@Temperature 23.9 °C
81.0 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have an excellent soft t..
Graves Tear Strength 14.2 kN/m

@Temperature 24.0 °C
81.0 pli

@Temperature 75.2 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ 6830 Thermoplastic Elastomer
With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte..