Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 1.40 g/cc
0.0325 - 0.0506 lb/in³
Average value: 1.17 g/cc Grade Count:832
0.935 - 1.02 g/cc

@Temperature 240 - 260 °C
0.0338 - 0.0368 lb/in³

@Temperature 464 - 500 °F
Average value: 0.981 g/cc Grade Count:16
Water Absorption 0.0100 - 0.700 %
0.0100 - 0.700 %
Average value: 0.313 % Grade Count:218
Moisture Absorption at Equilibrium 0.0100 - 8.00 %
0.0100 - 8.00 %
Average value: 0.222 % Grade Count:297
Water Absorption at Saturation 0.0800 - 1.00 %
0.0800 - 1.00 %
Average value: 0.420 % Grade Count:228
Viscosity 170000 - 195000 cP
170000 - 195000 cP
Average value: 187000 cP Grade Count:6
100000 - 195000 cP

@Temperature 260 - 260 °C
100000 - 195000 cP

@Temperature 500 - 500 °F
Average value: 204000 cP Grade Count:9
120000 - 480000 cP

@Temperature 260 - 260 °C
120000 - 480000 cP

@Temperature 500 - 500 °F
Average value: 204000 cP Grade Count:22
120000 - 480000 cP

@Shear Rate 1000 - 1000 1/s
120000 - 480000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 204000 cP Grade Count:22
Maximum Moisture Content 0.0100 - 0.0400
0.0100 - 0.0400
Average value: 0.0217 Grade Count:40
Linear Mold Shrinkage 0.000500 - 0.0140 cm/cm
0.000500 - 0.0140 in/in
Average value: 0.00563 cm/cm Grade Count:669
Linear Mold Shrinkage, Transverse 0.00150 - 0.0160 cm/cm
0.00150 - 0.0160 in/in
Average value: 0.00566 cm/cm Grade Count:137
Melt Flow 0.200 - 95.0 g/10 min
0.200 - 95.0 g/10 min
Average value: 17.1 g/10 min Grade Count:691
Spiral Flow 25.0 - 76.0 cm
9.84 - 29.9 in
Average value: 58.5 cm Grade Count:13
68.58 - 68.58 cm

@Temperature 260 - 260 °C
27.00 - 27.00 in

@Temperature 500 - 500 °F
Average value: 68.6 cm Grade Count:2
Mechanical Properties Metric English Comments
Hardness, Rockwell L 90.0
90.0
Average value: 90.0 Grade Count:6
Hardness, Rockwell M 72.0 - 97.0
72.0 - 97.0
Average value: 90.4 Grade Count:8
Hardness, Rockwell R 98.0 - 124
98.0 - 124
Average value: 115 Grade Count:222
Hardness, H358/30 89.0 - 121 MPa
12900 - 17500 psi
Average value: 104 MPa Grade Count:45
Hardness, Shore D 62.0
62.0
Average value: 62.0 Grade Count:3
Ball Indentation Hardness 85.0 - 105 MPa
12300 - 15200 psi
Average value: 96.3 MPa Grade Count:9
Tensile Strength, Ultimate 26.0 - 446 MPa
3770 - 64700 psi
Average value: 50.7 MPa Grade Count:470
20.0 - 45.0 MPa

@Temperature 60.0 - 90.0 °C
2900 - 6530 psi

@Temperature 140 - 194 °F
Average value: 32.5 MPa Grade Count:1
Tensile Strength, Yield 34.8 - 119 MPa
5050 - 17300 psi
Average value: 56.6 MPa Grade Count:724
Elongation at Break 1.25 - 220 %
1.25 - 220 %
Average value: 64.8 % Grade Count:665
45.0 - 55.0 %

@Temperature 60.0 - 90.0 °C
45.0 - 55.0 %

@Temperature 140 - 194 °F
Average value: 50.0 % Grade Count:1
Elongation at Yield 1.90 - 100 %
1.90 - 100 %
Average value: 5.15 % Grade Count:435
4.00 - 6.00 %

@Temperature 60.0 - 90.0 °C
4.00 - 6.00 %

@Temperature 140 - 194 °F
Average value: 5.00 % Grade Count:1
Modulus of Elasticity 1.67 - 10.3 GPa
242 - 1490 ksi
Average value: 2.75 GPa Grade Count:475
1.90 - 2.20 GPa

@Temperature 60.0 - 90.0 °C
276 - 319 ksi

@Temperature 140 - 194 °F
Average value: 2.05 GPa Grade Count:1
Flexural Yield Strength 8.20 - 159 MPa
1190 - 23100 psi
Average value: 88.9 MPa Grade Count:669
Flexural Modulus 0.290 - 12.9 GPa
42.1 - 1880 ksi
Average value: 2.60 GPa Grade Count:723
Izod Impact, Notched 0.196 - 56.0 J/cm
0.367 - 105 ft-lb/in
Average value: 5.18 J/cm Grade Count:628
0.380 - 6.40 J/cm

@Temperature -50.0 - 0.000 °C
0.712 - 12.0 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 2.90 J/cm Grade Count:224
1.01441 - 5.30 J/cm

@Temperature -40.0 - -10.0 °C
1.90041 - 9.93 ft-lb/in

@Temperature -40.0 - 14.0 °F
Average value: 2.90 J/cm Grade Count:39
1.01441 - 5.30 J/cm

@Thickness 3.17 - 6.35 mm
1.90041 - 9.93 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 2.90 J/cm Grade Count:39
Izod Impact, Unnotched 3.00 J/cm - NB
5.62 ft-lb/in - NB
Average value: 9.28 J/cm Grade Count:70
5.88 J/cm - NB

@Temperature -40.0 - -30.0 °C
11.0 ft-lb/in - NB

@Temperature -40.0 - -22.0 °F
Average value: 12.6 J/cm Grade Count:12
Izod Impact, Notched (ISO) 0.750 - 100 kJ/m²
0.357 - 47.6 ft-lb/in²
Average value: 35.1 kJ/m² Grade Count:287
0.590 - 61.0 kJ/m²

@Temperature -40.0 - 0.000 °C
0.281 - 29.0 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 19.0 kJ/m² Grade Count:242
Izod Impact, Unnotched (ISO) 21.0 kJ/m² - NB
9.99 ft-lb/in² - NB
Average value: 96.6 kJ/m² Grade Count:64
7.00 kJ/m² - NB

@Temperature -40.0 - -30.0 °C
3.33 ft-lb/in² - NB

@Temperature -40.0 - -22.0 °F
Average value: 66.2 kJ/m² Grade Count:25
Charpy Impact Unnotched 5.40 J/cm² - NB
25.7 ft-lb/in² - NB
Average value: 19.6 J/cm² Grade Count:55
4.90 J/cm² - NB

@Temperature -40.0 - -20.0 °C
23.3 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 21.6 J/cm² Grade Count:19
Charpy Impact, Notched 0.400 - 8.00 J/cm²
1.90 - 38.1 ft-lb/in²
Average value: 3.65 J/cm² Grade Count:276
0.300 - 5.00 J/cm²

@Temperature -40.0 - 0.000 °C
1.43 - 23.8 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 1.87 J/cm² Grade Count:213
Gardner Impact 27.1 - 37.0 J
20.0 - 27.3 ft-lb
Average value: 35.5 J Grade Count:11
Dart Drop, Total Energy 13.0 - 72.0 J
9.59 - 53.1 ft-lb
Average value: 52.3 J Grade Count:178
25.0 - 70.0 J

@Temperature -40.0 - -20.0 °C
18.4 - 51.6 ft-lb

@Temperature -40.0 - -4.00 °F
Average value: 52.3 J Grade Count:49
56.5 - 62.1 J

@Temperature -29.0 - -29.0 °C
41.7 - 45.8 ft-lb

@Temperature -20.2 - -20.2 °F
Average value: 52.3 J Grade Count:3
56.5 - 62.1 J

@Thickness 3.20 - 3.20 mm
41.7 - 45.8 ft-lb

@Thickness 0.126 - 0.126 in
Average value: 52.3 J Grade Count:3
Falling Dart Impact 6.78 - 54.2 J
5.00 - 40.0 ft-lb
Average value: 37.6 J Grade Count:6
50.1653 - 51.5212 J

@Temperature -28.9 - -28.9 °C
37.0000 - 38.0000 ft-lb

@Temperature -20.0 - -20.0 °F
Average value: 50.8 J Grade Count:2