Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Izod Impact, Notched | 1.06 - 6.40 J/cm | 1.99 - 12.0 ft-lb/in | colors; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains.. |
|||
Izod Impact, Notched | 2.14 - 6.41 J/cm | 4.00 - 12.0 ft-lb/in | Average value: 4.72 J/cm Grade Count:12 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Notched | 0.250 - 6.41 J/cm | 0.468 - 12.0 ft-lb/in | Average value: 1.05 J/cm Grade Count:69 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.380 - 6.40 J/cm @Temperature -50.0 - 0.000 °C |
0.712 - 12.0 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 2.90 J/cm Grade Count:224 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.801 - 6.41 J/cm | 1.50 - 12.0 ft-lb/in | Average value: 3.27 J/cm Grade Count:8 |
Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 2.67 - 6.41 J/cm | 5.00 - 12.0 ft-lb/in | Average value: 5.19 J/cm Grade Count:4 |
Overview of materials for Phenolic/Glass Fiber SMC This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Notched | 5.34 - 6.41 J/cm | 10.0 - 12.0 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 5.34 - 6.41 J/cm | 10.0 - 12.0 ft-lb/in | |
Bulk Molding Compounds BMC A50-XHS Bulk molding compound Description: BMC A50XHS is a high strength bulk molding compound. It can be supplied in bulk or extruded in preweighted slugs. Due to the excellent flow and controlled reactivity, BMC A50XHS i.. |
|||
Izod Impact, Notched | 5.34 - 6.41 J/cm | 10.0 - 12.0 ft-lb/in | |
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic.. |
|||
Izod Impact, Notched | 5.34 - 6.41 J/cm | 10.0 - 12.0 ft-lb/in | |
Bulk Molding Compounds BMC A50-XHS-U Bulk molding compound Description: BMC A50-XHS-U is a high strength bulk molding compound with a UL F1 rating for outdoor exposure. This material was specifically designed for outdoor lighting and electrical applications.. |
|||
Izod Impact, Notched | 1.07 - 6.41 J/cm | 2.00 - 12.0 ft-lb/in | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Izod Impact, Notched | 0.400 - 6.41 J/cm | 0.749 - 12.0 ft-lb/in | Average value: 1.15 J/cm Grade Count:22 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Izod Impact, Notched | 0.100 - 6.40 J/cm | 0.187 - 12.0 ft-lb/in | Average value: 2.22 J/cm Grade Count:309 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 0.267 - 6.41 J/cm | 0.500 - 12.0 ft-lb/in | Average value: 0.825 J/cm Grade Count:14 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Notched | 0.200 - 6.41 J/cm | 0.375 - 12.0 ft-lb/in | Average value: 0.959 J/cm Grade Count:58 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |