Physical Properties Metric English Comments
Spiral Flow 68.58 - 68.58 cm

@Temperature 260 - 260 °C
27.00 - 27.00 in

@Temperature 500 - 500 °F
Average value: 68.6 cm Grade Count:2
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..