Polymer Property : Tensile Strength, Yield = 119 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 - 119 MPa

@Temperature 100 - 175 °C
2900 - 17300 psi

@Temperature 212 - 347 °F
Average value: 64.8 MPa Grade Count:8
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Tensile Strength, Yield 65.5 - 119 MPa
9500 - 17300 psi
Average value: 90.8 MPa Grade Count:9
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..
Tensile Strength, Yield 27.6 - 119 MPa
4000 - 17300 psi
Average value: 57.1 MPa Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Tensile Strength, Yield 34.8 - 119 MPa
5050 - 17300 psi
Average value: 56.6 MPa Grade Count:724
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Tensile Strength, Yield 63.4 - 119 MPa

@Temperature 100 - 175 °C
9200 - 17300 psi

@Temperature 212 - 347 °F
Average value: 87.2 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are..