Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.900 - 5.00 J/cm² | 4.28 - 23.8 ft-lb/in² | Average value: 2.57 J/cm² Grade Count:19 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.300 - 5.00 J/cm² @Temperature -40.0 - 0.000 °C |
1.43 - 23.8 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 1.87 J/cm² Grade Count:213 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact, Notched | 0.500 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C |
2.38 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.79 J/cm² Grade Count:9 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 1.30 - 5.00 J/cm² | 6.19 - 23.8 ft-lb/in² | Average value: 3.01 J/cm² Grade Count:12 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Charpy Impact, Notched | 0.500 - 5.00 J/cm² | 2.38 - 23.8 ft-lb/in² | Average value: 2.02 J/cm² Grade Count:14 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Charpy Impact, Notched | 0.900 - 5.00 J/cm² @Temperature -30.0 - -20.0 °C |
4.28 - 23.8 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 3.24 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |
|||
Charpy Impact, Notched | 0.300 - 5.00 J/cm² | 1.43 - 23.8 ft-lb/in² | Average value: 2.44 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |