Polymer Property : Izod Impact, Notched = 6.40 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.06 - 6.40 J/cm
1.99 - 12.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HP1 PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release.
Izod Impact, Notched 1.06 - 6.40 J/cm
1.99 - 12.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HP1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount..
Izod Impact, Notched 1.06 - 6.40 J/cm
1.99 - 12.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HPS1 PC
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
Izod Impact, Notched 1.06 - 6.40 J/cm
1.99 - 12.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HPS1R PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont..
Izod Impact, Notched 1.06 - 6.40 J/cm
1.99 - 12.0 ft-lb/in
colors; ASTM D256
SABIC Innovative Plastics Lexan® HPS1R PC (Asia Pacific)
High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Contains..
Izod Impact, Notched 0.380 - 6.40 J/cm

@Temperature -50.0 - 0.000 °C
0.712 - 12.0 ft-lb/in

@Temperature -58.0 - 32.0 °F
Average value: 2.90 J/cm Grade Count:224
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.100 - 6.40 J/cm
0.187 - 12.0 ft-lb/in
Average value: 2.22 J/cm Grade Count:309
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..