Polymer Property : Izod Impact, Notched (ISO) = 100 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.80 - 100 kJ/m²
3.71 - 47.6 ft-lb/in²
Average value: 16.1 kJ/m² Grade Count:20
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Izod Impact, Notched (ISO) 0.750 - 100 kJ/m²
0.357 - 47.6 ft-lb/in²
Average value: 35.1 kJ/m² Grade Count:287
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..