Polymer Property : Ball Indentation Hardness = 85.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO2039.1 DIN.53456
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Acrylonitrile-butadiene-styrene is an amorphous thermopolymer used largely for injection moulded items. The stock shapes are mainly used for the production of prototypes.Features:Good machinability ..
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Ineos Nova S-6600 High Impact Compact Polystyrene  (discontinued **)
High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yogurt beakers but technical parts and extruded..
Ball Indentation Hardness 85.0 - 105 MPa
12300 - 15200 psi
Average value: 96.3 MPa Grade Count:9
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Ball Indentation Hardness 85.0 - 205 MPa
12300 - 29700 psi
Average value: 140 MPa Grade Count:3
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Ball Indentation Hardness 85.0 - 180 MPa
12300 - 26100 psi
Average value: 141 MPa Grade Count:11
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Global PP-1100-NK Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goods, closures, food applicationsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Global PP-1100-PK Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Global PP-1100-RC Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 85.0 MPa
12300 psi
DIN 53456
Global PP-1126-NK Polypropylene Homopolymer
Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation.
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade
Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles.
Ball Indentation Hardness 85.0 MPa

@Load 36.5 kg,
Time 30.0 sec
12300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 778 Q42 Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Ball Indentation Hardness 85.0 MPa

@Load 36.5 kg,
Time 30.0 sec
12300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 778 TE Black 25991 ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Ball Indentation Hardness 85.0 MPa

@Load 36.5 kg,
Time 30.0 sec
12300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 778 TE UV Colored ASA
Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Ball Indentation Hardness 85.0 MPa

@Load 36.5 kg,
Time 30.0 sec
12300 psi

@Load 80.5 lb,
Time 0.00833 hour
ISO 2039-1
Styrolution Luran® S 778 UV Colored ASA
Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan..
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Styrolution Novodur® 4105 ABS
Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Styrolution Novodur® 4140PG ABS
Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by ..
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Styrolution Novodur® E401 ABS
Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution
Ball Indentation Hardness 85.0 MPa
12300 psi
ISO 2039-1
Styrolution PS 476L HIPS
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl..
Ball Indentation Hardness 85.0 MPa
12300 psi
H 385/30; ISO 2039
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength..
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® AS/2 PA66
Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i..
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30
Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s..
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® BKZ-30 PA6-GB30
Information provided by EMS Grivory
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TSK-30/4 PA666-GB30
Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa..
Ball Indentation Hardness 85.0 MPa
12300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® TR 90 LXS PAMACM12
Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing..