Polymer Property : Izod Impact, Notched = 5.30 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.01441 - 5.30 J/cm

@Temperature -40.0 - -10.0 °C
1.90041 - 9.93 ft-lb/in

@Temperature -40.0 - 14.0 °F
Average value: 2.90 J/cm Grade Count:39
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 1.01441 - 5.30 J/cm

@Thickness 3.17 - 6.35 mm
1.90041 - 9.93 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 2.90 J/cm Grade Count:39
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 5.30 - 5.30 J/cm

@Temperature -10.0 - -10.0 °C
9.93 - 9.93 ft-lb/in

@Temperature 14.0 - 14.0 °F
Average value: 2.37 J/cm Grade Count:1
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 4.30 - 5.30 J/cm

@Temperature -29.0 - -29.0 °C
8.06 - 9.93 ft-lb/in

@Temperature -20.2 - -20.2 °F
Average value: 4.63 J/cm Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Izod Impact, Notched 0.530 - 5.30 J/cm
0.993 - 9.93 ft-lb/in
Average value: 2.12 J/cm Grade Count:5
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..
Izod Impact, Notched 0.300 - 5.30 J/cm
0.562 - 9.93 ft-lb/in
Average value: 1.17 J/cm Grade Count:27
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Izod Impact, Notched 0.310 - 5.30 J/cm
0.581 - 9.93 ft-lb/in
Average value: 0.762 J/cm Grade Count:14
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..