Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 25.0 - 70.0 J @Temperature -40.0 - -20.0 °C |
18.4 - 51.6 ft-lb @Temperature -40.0 - -4.00 °F |
Average value: 52.3 J Grade Count:49 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Dart Drop, Total Energy | 4.86739 - 70.0 J @Temperature -40.0 - -20.0 °C |
3.59000 - 51.6 ft-lb @Temperature -40.0 - -4.00 °F |
Average value: 51.3 J Grade Count:19 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |