Mechanical Properties Metric English Comments
Dart Drop, Total Energy 13.0 - 72.0 J
9.59 - 53.1 ft-lb
Average value: 52.3 J Grade Count:178
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..