Polymer Property : Modulus of Elasticity = 1.90 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.90 GPa
276 ksi
ISO 178
Premix Thermoplastics PRE-ELEC® PP 1380
PRE-ELEC PP 1380 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PR..
Modulus of Elasticity 1.90 GPa
276 ksi
ISO 527
GEHR Plastics PP-30PET-F Polypropylene, 30% PET Fiber Reinforced  (discontinued **)
Polypropylene shows a high mechanical strength and a tensile strength, but a low notched impact strength. PP resists stress cracking and it is easy to weld. At minus temperatures it can get brittle...
Modulus of Elasticity 1.90 GPa
276 ksi
DIN 53457
Ineos Nova S-6600 High Impact Compact Polystyrene  (discontinued **)
High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yot beakers but technical parts and extruded pr..
Modulus of Elasticity 1.90 - 2.06 GPa
276 - 299 ksi
Average value: 1.98 GPa Grade Count:9
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Modulus of Elasticity 1.90 - 2.20 GPa

@Temperature 60.0 - 90.0 °C
276 - 319 ksi

@Temperature 140 - 194 °F
Average value: 2.05 GPa Grade Count:1
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Modulus of Elasticity 1.90 - 9.00 GPa

@Temperature 50.0 - 200 °C
276 - 1310 ksi

@Temperature 122 - 392 °F
Average value: 7.30 GPa Grade Count:7
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Modulus of Elasticity 1.90 GPa
276 ksi
Youngs Modulus, ASTM D638, 10%/min.
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p..
Modulus of Elasticity 1.90 - 9.31 GPa
276 - 1350 ksi
Average value: 5.50 GPa Grade Count:21
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Modulus of Elasticity 1.90 GPa
276 ksi
ASTM D638
Spartech Royalite R632M Carbon Black Filled ABS/PVC Resin
Data provided by the manufacturer. This static-conductive material is UL®-listed and meets minimum static-decay requirements outlined in MIL-B-1705B and NFPA Code 56A specifications.
Modulus of Elasticity 1.90 GPa
276 ksi
Conditioned; ISO 178
Addiplast Addinyl B2 1 Flame Retardant Nylon 6
Flame retardant, halogen freeInformation provided by Addiplast.
Modulus of Elasticity 1.90 GPa
276 ksi
DIN EN ISO 527
BASF Elastollan R 2005/1 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Modulus of Elasticity 1.90 GPa
275 ksi
Machine; ASTM D638
Arlon CuClad 217 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 217 uses a low fiberglass/PTFE ratio to provide the lowest dielectric constant and dissipation factor available in fiberglass reinforced PTFE based laminates. Together, these properties offe..
Modulus of Elasticity 1.90 GPa

@Temperature 60.0 °C
276 ksi

@Temperature 140 °F
ISO 899-1
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
Modulus of Elasticity 1.90 GPa
276 ksi
ISO 178
Addiplast Addinyl C2 R Nylon 66/6
High impact resistanceInformation provided by Addiplast.
Modulus of Elasticity 1.90 GPa
276 ksi
ISO 527-2
BASF Ultraform® N2650 Z2 (LEV) POM
Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr..
Modulus of Elasticity 1.90 - 16.0 GPa
276 - 2320 ksi
Average value: 4.99 GPa Grade Count:57
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Modulus of Elasticity 1.90 GPa
276 ksi
Youngs Modulus, ASTM D638, 10%/min.
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..