GRECO ISOPAK 547SHF ABS Resin

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer GRECO
Trade Name ISOPAK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF GRECO ISOPAK 547SHF ABS Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact and High Flow GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength 37.3 MPa
5400 psi
ASTM D638
Flexural Yield Strength 65.7 MPa
9530 psi
ASTM D790
Izod Impact, Notched 2.84 J/cm
5.33 ft-lb/in
ASTM D256 A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ASTM D648
Flammability, UL94 HB
HB