Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.67 - 10.3 GPa | 242 - 1490 ksi | Average value: 2.75 GPa Grade Count:475 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |