Polymer Property : Charpy Impact, Notched = 5.00 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.900 - 5.00 J/cm²
4.28 - 23.8 ft-lb/in²
Average value: 2.57 J/cm² Grade Count:19
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Charpy Impact, Notched 0.300 - 5.00 J/cm²

@Temperature -40.0 - 0.000 °C
1.43 - 23.8 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 1.87 J/cm² Grade Count:213
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Charpy Impact, Notched 0.500 - 5.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.79 J/cm² Grade Count:9
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 1.30 - 5.00 J/cm²
6.19 - 23.8 ft-lb/in²
Average value: 3.01 J/cm² Grade Count:12
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl..
Charpy Impact, Notched 0.500 - 5.00 J/cm²
2.38 - 23.8 ft-lb/in²
Average value: 2.02 J/cm² Grade Count:14
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..
Charpy Impact, Notched 0.900 - 5.00 J/cm²

@Temperature -30.0 - -20.0 °C
4.28 - 23.8 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 3.24 J/cm² Grade Count:8
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..
Charpy Impact, Notched 0.300 - 5.00 J/cm²
1.43 - 23.8 ft-lb/in²
Average value: 2.44 J/cm² Grade Count:8
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..