Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.90 J/cm²

@Temperature -30.0 °C
23.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific)
Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications.
Charpy Impact Unnotched 4.90 J/cm²

@Temperature -30.0 °C
23.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4413 PC
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 4.90 J/cm²

@Temperature -30.0 °C
23.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4413 PC (Asia Pacific)
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Charpy Impact Unnotched 4.90 J/cm²
23.3 ft-lb/in²
ISO 179/1eU
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Charpy Impact Unnotched 4.90 J/cm² - NB

@Temperature -40.0 - -20.0 °C
23.3 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 21.6 J/cm² Grade Count:19
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Charpy Impact Unnotched 4.90 J/cm²
23.3 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Charpy Impact Unnotched 4.90 J/cm²
23.3 ft-lb/in²
ISO 179/1eU
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab..
Charpy Impact Unnotched 4.90 J/cm²

@Temperature -30.0 °C
23.3 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics Lexan® HFD4413 PC (Europe-Africa-Middle East)
Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Copyright © lookpolymers.com All Rights Reserved