Polymer Property : Izod Impact, Notched = 1.01441 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.01441 - 5.30 J/cm

@Temperature -40.0 - -10.0 °C
1.90041 - 9.93 ft-lb/in

@Temperature -40.0 - 14.0 °F
Average value: 2.90 J/cm Grade Count:39
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 1.01441 - 5.30 J/cm

@Thickness 3.17 - 6.35 mm
1.90041 - 9.93 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 2.90 J/cm Grade Count:39
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 1.01441 - 1.01441 J/cm

@Temperature -40.0 - -40.0 °C
1.90041 - 1.90041 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 2.55 J/cm Grade Count:1
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Izod Impact, Notched 1.01441 - 1.01441 J/cm

@Thickness 3.17 - 3.17 mm
1.90041 - 1.90041 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 2.55 J/cm Grade Count:1
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Izod Impact, Notched 1.01441 - 1.01441 J/cm

@Temperature -40.0 - -40.0 °C
1.90041 - 1.90041 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.01 J/cm Grade Count:1
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 1.01441 - 1.01441 J/cm

@Thickness 3.17 - 3.17 mm
1.90041 - 1.90041 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.01 J/cm Grade Count:1
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 1.01441 - 1.33475 J/cm

@Temperature -40.0 - -40.0 °C
1.90041 - 2.50053 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.20 J/cm Grade Count:7
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..