Mechanical Properties Metric English Comments
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY CR7020 ASA
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific)
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 505RU PC
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific)
Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro..
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East)
Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE..
Dart Drop, Total Energy 25.0 - 70.0 J

@Temperature -40.0 - -20.0 °C
18.4 - 51.6 ft-lb

@Temperature -40.0 - -4.00 °F
Average value: 52.3 J Grade Count:49
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Dart Drop, Total Energy 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
Instrumented; ASTM D3763
LyondellBasell Hifaxâ„¢ CA244 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic..
Dart Drop, Total Energy 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
Instrumented; ASTM D3763
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer
Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint..
Dart Drop, Total Energy 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of ..
Dart Drop, Total Energy 25.0 J

@Temperature 0.000 °C
18.4 ft-lb

@Temperature 32.0 °F
Instrumented Energy at Maximum Load; ASTM D3763
LyondellBasell Hostacomâ„¢ TKS708D Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ TKS708D medium high melt flow, 1,300 MPa flexural modulus, UV-stabilized, high impact thermoplastic elastomeric olefin (TEO) resin has an excellent combination of propert..
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DEI13F PC (Asia Pacific)
LNP* Stat-kon* DEI13F is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Internally Lu..
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX05499 PC
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific)
LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Valox® HX3061HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6
LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6
LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific)
LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON DEI13F PC
LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R..
Dart Drop, Total Energy 25.0 J
18.4 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific)
LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6
Compound based on Nylon 6 resin containing glass fiber and impact modifier.
Dart Drop, Total Energy 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics NORYL EM6101 PPE+PS
Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range.
Dart Drop, Total Energy 25.0 J

@Thickness 0.0500 mm
18.4 ft-lb

@Thickness 0.00197 in
1100 N force; ISO 7765-2
Borealis BA11CF Polypropylene Copolymer
BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. ..
Dart Drop, Total Energy 25.0 J

@Thickness 0.0500 mm
18.4 ft-lb

@Thickness 0.00197 in
1200N; ISO 7765-2
Borealis Borseal™ RE239CF Polypropylene Copolymer
Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high..
Dart Drop, Total Energy 24.9 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3763
ExxonMobil Exxtral™ H1025W Performance Polyolefin
Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive..
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific)
ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL.
Dart Drop, Total Energy 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC
LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.