Physical Properties Metric English Comments
Viscosity 170000 cP

@Temperature 260 °C
170000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region.
Viscosity 170000 cP

@Temperature 260 °C
170000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region.
Viscosity 170000 cP

@Temperature 260 °C
170000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
Viscosity 170000 cP
170000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Viscosity 170000 cP
170000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Viscosity 170000 cP

@Temperature 260 °C
170000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East)
PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur..
Viscosity 170000 cP

@Shear Rate 60.0 1/s,
Temperature 200 °C
170000 cP

@Shear Rate 60.0 1/s,
Temperature 392 °F
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer
Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n..
Viscosity 170000 cP

@Temperature 130 °C
170000 cP

@Temperature 266 °F
Melt; DIN 53.735
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde..
Viscosity 170000 - 195000 cP
170000 - 195000 cP
Average value: 187000 cP Grade Count:6
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Viscosity 170000 - 1.40e+7 cP

@Temperature 200 - 230 °C
170000 - 1.40e+7 cP

@Temperature 392 - 446 °F
Average value: 1.29e+6 cP Grade Count:11
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Viscosity 170000 - 1.40e+7 cP

@Shear Rate 60.0 - 270 1/s
170000 - 1.40e+7 cP

@Shear Rate 60.0 - 270 1/s
Average value: 1.29e+6 cP Grade Count:11
Overview of materials for Ethylene Vinyl Alcohol (EVOH)
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr..
Viscosity 170000 cP
170000 cP
"A" component
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating  (discontinued **)
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem..
Viscosity 170000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
170000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear..
Viscosity 170000 cP
170000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East)
VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles.
Viscosity 170000 cP
170000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Viscosity 170000 cP
170000 cP
Elmer's Products Aron Alpha® GEL 10 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
Viscosity 170000 cP

@Temperature 160 °C
170000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 170000 cP
170000 cP
Mixed
Armstrong A-2/E Epoxy Adhesive
This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac..