Physical Properties Metric English Comments
Melt Flow 0.200 - 26.0 g/10 min
0.200 - 26.0 g/10 min
Average value: 5.91 g/10 min Grade Count:136
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..
Melt Flow 0.200 - 10.0 g/10 min
0.200 - 10.0 g/10 min
Average value: 1.86 g/10 min Grade Count:5
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Melt Flow 0.200 - 95.0 g/10 min
0.200 - 95.0 g/10 min
Average value: 17.1 g/10 min Grade Count:691
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Melt Flow 0.200 - 1200 g/10 min
0.200 - 1200 g/10 min
Average value: 23.4 g/10 min Grade Count:842
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Melt Flow 0.200 - 1.10 g/10 min
0.200 - 1.10 g/10 min
Average value: 0.660 g/10 min Grade Count:5
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Melt Flow 0.200 - 10.0 g/10 min
0.200 - 10.0 g/10 min
Average value: 3.72 g/10 min Grade Count:14
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Melt Flow 0.200 - 21.0 g/10 min
0.200 - 21.0 g/10 min
Average value: 5.24 g/10 min Grade Count:13
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is ..
Melt Flow 0.200 - 42.0 g/10 min
0.200 - 42.0 g/10 min
Average value: 7.67 g/10 min Grade Count:125
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Melt Flow 0.200 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.200 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1688A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 2419C Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4670A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1025-65 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1025-72 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; Closures; General Purpose; Grommets; Weatherstripping Forms:..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1035-70UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-87-L832-B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-89-P808A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 0.200 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.200 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TELC 1025-70 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 0.200 - 12.0 g/10 min
0.200 - 12.0 g/10 min
Average value: 1.39 g/10 min Grade Count:75
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Melt Flow 0.200 - 155 g/10 min
0.200 - 155 g/10 min
Average value: 48.3 g/10 min Grade Count:27
Overview of materials for Low Density Polyethylene (LDPE), Masterbatch Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Masterbatch Grade". Each property range of values reported is minimum a..
Melt Flow 0.200 - 123 g/10 min
0.200 - 123 g/10 min
Average value: 3.51 g/10 min Grade Count:241
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Melt Flow 0.200 - 21.0 g/10 min
0.200 - 21.0 g/10 min
Average value: 3.84 g/10 min Grade Count:22
Overview of materials for Medium Density Polyethylene (MDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max..
Melt Flow 0.200 - 30.0 g/10 min
0.200 - 30.0 g/10 min
Average value: 5.94 g/10 min Grade Count:79
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
Melt Flow 0.200 - 150 g/10 min
0.200 - 150 g/10 min
Average value: 18.2 g/10 min Grade Count:900
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..