Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.00 - 1.16 g/cc
0.0361 - 0.0419 lb/in³
Average value: 1.08 g/cc Grade Count:128
Water Absorption 0.300 - 1.65 %
0.300 - 1.65 %
Average value: 0.923 % Grade Count:11
Moisture Absorption at Equilibrium 0.150 - 0.350 %
0.150 - 0.350 %
Average value: 0.249 % Grade Count:20
Water Absorption at Saturation 0.500 - 1.00 %
0.500 - 1.00 %
Average value: 0.620 % Grade Count:15
Maximum Moisture Content 0.0100
0.0100
Average value: 0.0100 Grade Count:11
Linear Mold Shrinkage 0.000 - 0.0100 cm/cm
0.000 - 0.0100 in/in
Average value: 0.00531 cm/cm Grade Count:104
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00654 cm/cm Grade Count:13
Melt Flow 0.200 - 42.0 g/10 min
0.200 - 42.0 g/10 min
Average value: 7.67 g/10 min Grade Count:125
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80.0 - 119
80.0 - 119
Average value: 100 Grade Count:76
Tensile Strength, Ultimate 25.0 - 75.5 MPa
3630 - 11000 psi
Average value: 39.2 MPa Grade Count:34
Tensile Strength, Yield 20.7 - 58.3 MPa
3000 - 8450 psi
Average value: 44.5 MPa Grade Count:118
13.0 - 79.0 MPa

@Temperature -40.0 - 80.0 °C
1890 - 11500 psi

@Temperature -40.0 - 176 °F
Average value: 45.9 MPa Grade Count:5
Elongation at Break 3.00 - 230 %
3.00 - 230 %
Average value: 31.9 % Grade Count:79
Elongation at Yield 2.50 - 6.00 %
2.50 - 6.00 %
Average value: 3.36 % Grade Count:51
1.90 - 5.10 %

@Temperature -40.0 - 80.0 °C
1.90 - 5.10 %

@Temperature -40.0 - 176 °F
Average value: 3.45 % Grade Count:5
Modulus of Elasticity 1.45 - 2.85 GPa
210 - 413 ksi
Average value: 2.28 GPa Grade Count:59
Flexural Yield Strength 40.7 - 115 MPa
5900 - 16600 psi
Average value: 69.4 MPa Grade Count:77
Flexural Modulus 1.34 - 3.17 GPa
195 - 460 ksi
Average value: 2.27 GPa Grade Count:111
Izod Impact, Notched 0.320 - 5.87 J/cm
0.600 - 11.0 ft-lb/in
Average value: 1.80 J/cm Grade Count:106
0.230 - 0.570 J/cm

@Temperature -40.0 - -30.0 °C
0.431 - 1.07 ft-lb/in

@Temperature -40.0 - -22.0 °F
Average value: 0.377 J/cm Grade Count:22
0.196133 - 1.07 J/cm

@Temperature -30.0 - -30.0 °C
0.367438 - 2.00 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.377 J/cm Grade Count:11
0.196133 - 1.07 J/cm

@Thickness 3.17 - 6.40 mm
0.367438 - 2.00 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 0.377 J/cm Grade Count:11
Izod Impact, Notched (ISO) 5.00 - 42.0 kJ/m²
2.38 - 20.0 ft-lb/in²
Average value: 12.6 kJ/m² Grade Count:28
2.00 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.25 kJ/m² Grade Count:24
Izod Impact, Unnotched (ISO) 80.0 - 100 kJ/m²
38.1 - 47.6 ft-lb/in²
Average value: 85.0 kJ/m² Grade Count:4
40.0 - 45.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 21.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 41.3 kJ/m² Grade Count:4
Charpy Impact Unnotched 8.00 J/cm² - NB
38.1 ft-lb/in² - NB
Average value: 13.9 J/cm² Grade Count:10
4.00 - 9.00 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.47 J/cm² Grade Count:10
Charpy Impact, Notched 0.700 - 5.77 J/cm²
3.33 - 27.5 ft-lb/in²
Average value: 1.88 J/cm² Grade Count:35
0.110 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
0.524 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.507 J/cm² Grade Count:20
Dart Drop, Total Energy 15.0 - 56.0 J
11.1 - 41.3 ft-lb
Average value: 39.5 J Grade Count:4
Tensile Creep Modulus, 1000 hours 1250 - 1650 MPa
181000 - 239000 psi
Average value: 1430 MPa Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 7.90 - 121 µm/m-°C
4.39 - 67.2 µin/in-°F
Average value: 92.5 µm/m-°C Grade Count:43
CTE, linear, Transverse to Flow 86.4 - 130 µm/m-°C
48.0 - 72.2 µin/in-°F
Average value: 101 µm/m-°C Grade Count:25
Hot Ball Pressure Test 90.0 - 95.0 °C
194 - 203 °F
Average value: 93.3 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 106 °C
176 - 223 °F
Average value: 94.3 °C Grade Count:52
Deflection Temperature at 1.8 MPa (264 psi) 39.4 - 115 °C
103 - 239 °F
Average value: 86.3 °C Grade Count:118
Vicat Softening Point 78.0 - 133 °C
172 - 271 °F
Average value: 97.6 °C Grade Count:117
UL RTI, Electrical 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:5
UL RTI, Mechanical with Impact 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:5
UL RTI, Mechanical without Impact 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:5
Flammability, UL94 HB
HB
Grade Count:46
Oxygen Index 19.0 %
19.0 %
Average value: 19.0 % Grade Count:6
Glow Wire Test 750 °C
1380 °F
Average value: 750 °C Grade Count:5
Optical Properties Metric English Comments
Haze 6.00 - 8.00 %
6.00 - 8.00 %
Average value: 7.20 % Grade Count:3
Gloss 21.0 - 96.5 %
21.0 - 96.5 %
Average value: 82.8 % Grade Count:16
Transmission, Visible 85.5 - 88.0 %
85.5 - 88.0 %
Average value: 87.2 % Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+12 - 1.00e+15 ohm-cm
1.00e+12 - 1.00e+15 ohm-cm
Average value: 1.58e+14 ohm-cm Grade Count:14
Surface Resistance 1.10e+11 - 1.00e+15 ohm
1.10e+11 - 1.00e+15 ohm
Average value: 1.44e+14 ohm Grade Count:8
Dielectric Constant 3.20 - 5.20
3.20 - 5.20
Average value: 3.65 Grade Count:6
Dielectric Strength 15.7 - 35.0 kV/mm
400 - 889 kV/in
Average value: 27.6 kV/mm Grade Count:10
Dissipation Factor 0.00900 - 0.150
0.00900 - 0.150
Average value: 0.0266 Grade Count:8
Arc Resistance 60.0 - 180 sec
60.0 - 180 sec
Average value: 105 sec Grade Count:4
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:6
Hot Wire Ignition, HWI 3.00 - 60.0 sec
3.00 - 60.0 sec
Average value: 18.6 sec Grade Count:6
High Amp Arc Ignition, HAI 0.000 - 120 arcs
0.000 - 120 arcs
Average value: 102 arcs Grade Count:6
Users viewing this material also viewed the following: