Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.00 - 16.0 kJ/m² | 3.81 - 7.61 ft-lb/in² | Average value: 10.7 kJ/m² Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Average value: 8.14 kJ/m² Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched (ISO) | 14.0 - 16.0 kJ/m² @Temperature -30.0 - -30.0 °C |
6.66 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 17.5 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 14.0 - 16.0 kJ/m² @Thickness 3.20 - 3.20 mm |
6.66 - 7.61 ft-lb/in² @Thickness 0.126 - 0.126 in |
Average value: 17.5 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 16.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.71 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 13.4 kJ/m² Grade Count:17 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 16.0 kJ/m² @Thickness 3.20 - 3.20 mm |
5.71 - 7.61 ft-lb/in² @Thickness 0.126 - 0.126 in |
Average value: 13.4 kJ/m² Grade Count:17 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched (ISO) | 3.80 - 16.0 kJ/m² | 1.81 - 7.61 ft-lb/in² | Average value: 7.07 kJ/m² Grade Count:7 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 16.0 kJ/m² | 3.81 - 7.61 ft-lb/in² | Average value: 10.9 kJ/m² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 16.0 kJ/m² @Temperature -30.0 - -30.0 °C |
0.952 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.25 kJ/m² Grade Count:24 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched (ISO) | 2.40 - 16.0 kJ/m² | 1.14 - 7.61 ft-lb/in² | Average value: 5.97 kJ/m² Grade Count:55 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 16.0 kJ/m² | 2.86 - 7.61 ft-lb/in² | Average value: 10.2 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Izod Impact, Notched (ISO) | 3.50 - 16.0 kJ/m² | 1.67 - 7.61 ft-lb/in² | Average value: 8.10 kJ/m² Grade Count:55 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Izod Impact, Notched (ISO) | 1.60 - 16.0 kJ/m² | 0.761 - 7.61 ft-lb/in² | Average value: 6.02 kJ/m² Grade Count:33 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched (ISO) | 2.60 - 16.0 kJ/m² | 1.24 - 7.61 ft-lb/in² | Average value: 5.20 kJ/m² Grade Count:31 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 16.0 kJ/m² @Temperature -30.0 - -30.0 °C |
5.71 - 7.61 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 15.1 kJ/m² Grade Count:36 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 12.0 - 16.0 kJ/m² @Thickness 3.20 - 3.20 mm |
5.71 - 7.61 ft-lb/in² @Thickness 0.126 - 0.126 in |
Average value: 15.1 kJ/m² Grade Count:36 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 4.00 - 16.0 kJ/m² @Temperature -30.0 - -18.0 °C |
1.90 - 7.61 ft-lb/in² @Temperature -22.0 - -0.400 °F |
Average value: 8.77 kJ/m² Grade Count:39 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 6.50 - 16.0 kJ/m² | 3.09 - 7.61 ft-lb/in² | Average value: 11.0 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched (ISO) | 4.60 - 16.0 kJ/m² @Temperature -40.0 - -20.0 °C |
2.19 - 7.61 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 8.37 kJ/m² Grade Count:15 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |