Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 41.0 - 133 °C | 106 - 271 °F | Average value: 117 °C Grade Count:51 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Vicat Softening Point | 78.0 - 133 °C | 172 - 271 °F | Average value: 97.6 °C Grade Count:117 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |