Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Premix Thermoplastics PRE-ELEC® PP 1395 PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Advanced Elastomer Systems VistaFlex® 714-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Polykemi AB POLYfill PPH GF5015 PD1 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Ineos ABS Centrex® 601 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionInformation.. |
|||
Density | 1.00 - 1.16 g/cc | 0.0361 - 0.0419 lb/in³ | Average value: 1.08 g/cc Grade Count:128 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D1505 |
Micropol Microlink XL28/FR Black Crosslinkable Polyethylene Flame retardant. Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact),.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
LATI Latistat 47/7-03 PP Copolymer Dissipative product based on Polypropylene copolymer (PPc). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Heraeus Cleviosâ„¢ PH 500 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 500 is an antistatic material based on PEDO.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON MD000I PP (Europe-Africa-Middle East) LNP* Stat-kon* MD000I is a compound based on Polypropylene resin. Added features of this material include: Electrically Conductive, High Impact. |
|||
Density | 1.00 - 1.04 g/cc | 0.0361 - 0.0376 lb/in³ | RP-0549 |
Solvay AG-RHOâ„¢ FM 3896 Surfactant Description: Agricultural Foam Marker Concentrate. Very low alcohol content. Performs well in hard water up to 1000 ppmChemical Name: FOAM MARKER CONCENTRATE CAS: 111-76-2, 64-17-5 Solubility in Wat.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Solvay ALKAMULS® AP Surfactant Description: Ethoxylated oleic acid with low free PEG contentIdentification: ETHOXYLATED OLEIC ACIDCAS: 9004 – 96 – 0Available in: Asia Pacific, Europe, Latin America Solubility: Dispersib.. |
|||
Density | 1.00 - 1.15 g/cc | 0.0361 - 0.0415 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America EM 7400-2 Long Glass Fiber Reinforced Epoxy EM 7400-2 is a polyaramide fiber reinforced epoxy molding compound, which features abrasion resistance and light weight.Information provided by Sumitomo Bakelite North America, Inc. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Solvay RHODASURF® L-7/90 Surfactant Chemical Name: NONIONIC EMULSIFIERAvailable in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF© L 7 90 is an excellent primary nonionic surfactant recommended espec.. |
|||
Density | >= 1.00 g/cc | >= 0.0361 lb/in³ | |
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate Description: Specialty monomer for Rheology modificationChemical Name: POLYALKOXYL POLYARYLPHENOL ETHYLENIC METHACRYLATECAS: 79-41-4Available in: Asia Pacific, Europe, Latin America and North Americ.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Washington Penn High Modulus Polypropylene Copolymer 15% Mica Filled Mica-filled polypropylene compounds provide the best strength and modulus of any of the particulate fillers which results in an outstanding balance of properties. Mold shrinkage is similar to ABS a.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® TU-906 Two-Component Polyurethane Flexible Encapsulant Emerson & Cuming TU-906 Stycast® Two-Component Polyurethane Flexible EncapsulantDescriptionGood thermal shock and moisture resistance. Good chemical resistance. Low viscosity. Mix Ratio (by weight).. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Eliokem Chemigum® P83 Nitrile Elastomer Balanced modifier of plasticized PVC for improved properties and melt processing in the Eliokem product line. 33% bound ACN. Crosslinked polymer structure. PVC partitioning agent.Can be used in P.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® TR 90 UV PAMACM12 Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding propert.. |
|||
Density | 1.00 g/cc @Temperature 15.0 °C |
0.0361 lb/in³ @Temperature 59.0 °F |
|
ExxonMobil Kutwell 82 KUTWELL is the trademark for a line of two high-performance "soluble" cutting fluids for cooling and lubricating the tool and work in machining operations. The line includes one petroleum-base fluid.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
BASF Procom® D 1173 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
A.D. Compound Adene NC180A Homopolymer 15% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PP FR BK Availability: North AmericaForms: PelletsFeature: Flame Retardant, Homopolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Density | 1.00 - 2.20 g/cc | 0.0361 - 0.0795 lb/in³ | Average value: 1.76 g/cc Grade Count:71 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | |
Solvay RHODASURF® ON-877 Surfactant Description: Rhodasurf® ON 877 is Ethoxylated Oleyl Alcohol. It is excellent emulsifier, wetting agent, dispersant, and detergentChemical Name: ETHOXYLATED OLEYL ALCOHOLCAS: 68526-94-3Available in:.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® BRZ 334 H PA6 Product description: Grilon BRZ 334 H is a heat stabilized, medium viscosity, high impact modified PA6 extrusion grade. Grilon BRZ 334 H has the following important properties:High impact strength a.. |
|||
Density | 1.00 g/cc | 0.0361 lb/in³ | ISO 1183 |
Polyplastic TechnoTep A® 65 A Thermoplastic Elastomer, Mineral Filled Low mineral filled, good flexibilityInformation provided by PolyPlastic Group. |