Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 7.61 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.300 - 1.60 J/cm²

@Temperature -40.0 - 30.0 °C
1.43 - 7.61 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 0.901 J/cm² Grade Count:89
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.396 J/cm² Grade Count:23
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.50 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.50 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.55 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.55 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 1.20 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.62 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact, Notched 1.20 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
5.71 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.62 J/cm² Grade Count:4
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.44 J/cm² Grade Count:16
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 1.40 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.44 J/cm² Grade Count:16
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.110 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
0.524 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.507 J/cm² Grade Count:20
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.682 J/cm² Grade Count:83
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.600 - 1.60 J/cm²
2.86 - 7.61 ft-lb/in²
Average value: 0.872 J/cm² Grade Count:8
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.569 J/cm² Grade Count:28
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact, Notched 0.800 - 1.60 J/cm²

@Temperature -30.0 - 0.000 °C
3.81 - 7.61 ft-lb/in²

@Temperature -22.0 - 32.0 °F
Average value: 1.23 J/cm² Grade Count:3
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Charpy Impact, Notched 0.300 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
1.43 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.789 J/cm² Grade Count:60
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Charpy Impact, Notched 0.850 - 1.60 J/cm²
4.05 - 7.61 ft-lb/in²
Average value: 1.06 J/cm² Grade Count:14
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Copyright © lookpolymers.com All Rights Reserved